Reference health

Joining of ZrB <sub>2</sub> ‐Based Ultra‐High‐Temperature Ceramic Composites to Cu–Clad–Molybdenum for Advanced Aerospace Applications

https://doi.org/10.1111/j.1744-7402.2008.02291.x
CiteStamped reference-health badge
16/16 checkable references clean · checked 2026-07-23

Every reference with a DOI in the deposited reference list resolved to a known work in Crossref or DataCite at the dated check, and none carried a retraction, withdrawal, or removal notice.

9 without a DOI — not checked. A reference deposited without a DOI is never matched by title or guessed at; it stays outside the checked set, and this line discloses that.

The 16 checked references that resolve
resolves10.1016/S1369-7021(06)71635-2
Fraunhofer: a scientific/technical icon
resolves10.1016/S0955-2219(02)00140-1
Evaluation of ultra-high temperature ceramics foraeropropulsion use
resolves10.1111/j.1551-2916.2006.00999.x
Properties of a Pressureless‐Sintered ZrB <sub>2</sub> –MoSi <sub>2</sub> Ceramic Composite
resolves10.1016/S0955-2219(01)00284-9
Processing and properties of zirconium diboride-based composites
resolves10.1111/j.1151-2916.2000.tb01558.x
Reactive Hot Pressing of ZrB <sub>2</sub> –SiC Composites
resolves10.1016/j.msea.2007.01.015
Joining of zirconium diboride-based ultra high-temperature ceramic composites using metallic glass interlayers
resolves10.1111/j.1744-7402.2007.02126.x
Brazing of Stainless Steel to Yttria‐Stabilized Zirconia Using Gold‐Based Brazes for Solid Oxide Fuel Cell Applications
resolves10.1016/j.jeurceramsoc.2007.06.017
Joining of partially sintered alumina to alumina, titanium, Hastealloy and C–SiC composite using Ag–Cu brazes
resolves10.1016/j.msea.2005.08.179
Active metal brazing and characterization of brazed joints in titanium to carbon–carbon composites
resolves10.1016/j.msea.2005.10.067
A simple test to determine the effectiveness of different braze compositions for joining Ti-tubes to C/C composite plates
resolves10.1007/s10853-005-1948-1
Wetting and spreading of liquid metals on ZrB2-based ceramics
resolves10.1007/s10853-006-0442-8
Wetting of Group IV diborides by liquid metals
resolves10.1007/978-1-4757-3912-1
Composite Materials
resolves10.1016/S1359-6454(01)00352-4
Strain energy distribution in ceramic-to-metal joints
resolves10.1016/j.scriptamat.2003.09.055
Strain energy release in ceramic-to-metal joints with patterned interlayers
resolves10.1016/j.scriptamat.2005.06.001
Strain energy release in ceramic-to-metal joints by ductile metal interlayers
The 9 references without a DOI — listed, not checked
no DOI — not checkedSynthesis of Oxidation‐Resistant Metal Diboride Composites
no DOI — not checkedRefractory Diborides as Engineering Materials
no DOI — not checkedA.BellosiandF.Monteverde“Fabrication and Properties of Zirconium Diboride‐Based Ceramics for UHT Applications ”Proceedings of the 4th European Workshop on Hot Structures and Thermal Protection Systems for Space Vehicles Palermo Italy November 26–29 2002 (ESA SP‐521) April 2003.
no DOI — not checkedProperties of Ceramics in the ZrB2/ZrC/SiC System Prepared by Reactive Processing
no DOI — not checkedProceedings of the 9th International Symposium on Materials in a Space Environment, June 2003, Noordwijk, The Netherlands, ESA SP‐540
no DOI — not checkedElectronic Materials and Processes Handbook
no DOI — not checkedMetal–Ceramic Interfaces
no DOI — not checkede_1_2_7_21_2
no DOI — not checkedProperties of Advanced Semiconductor Materials GaN, AlN, SiC, BN, SiC, SiGe
What this badge says. CiteStamped means the CHECKABLE references of this work were clean at the dated check: each resolved to a known work in a public registry, and none carried a retraction notice at that time. It says nothing about the quality, findings, or importance of the work itself, and nothing about references deposited without a DOI.

checked 2026-07-23 — re-checked daily as this page is visited; titles and statuses come from Crossref and DataCite and are not part of the signed record

Embed this badge

Both snippets point at the live badge image and link back to this page. The badge re-renders from the daily check, so an embed never goes stale by more than a day of visits.

<a href="https://citestamp.com/citestamped/10.1111/j.1744-7402.2008.02291.x"><img src="https://citestamp.com/citestamped/10.1111/j.1744-7402.2008.02291.x/badge.svg" alt="CiteStamped reference-health badge" width="460" height="64"></a>
[![CiteStamped reference-health badge](https://citestamp.com/citestamped/10.1111/j.1744-7402.2008.02291.x/badge.svg)](https://citestamp.com/citestamped/10.1111/j.1744-7402.2008.02291.x)