On the public citation graph

Gaseous hydrogen embrittlement of high strength steels

0 signed · 197 inferred · view as graph

Inferred edges come from two machine sources: sweeps of open repository metadata (mostly SSRN and Zenodo), and a bulk OpenAlex citation snapshot. Every row below is labelled with the one it came from. Neither is a complete citation index — absence here is not evidence of absence.

Is this your work? Sign in with ORCID and put your name on the claims that are yours.
Claim with ORCID
Reference health. See whether every reference in this work resolves to a known work and none has been retracted — and get a dated CiteStamped badge you can embed.
See reference health

What this work says

Outgoing claims: the papers this work cites, builds on, or argues with.

inferredcites →https://doi.org/10.1002/bbpc.19720760864openalex-snapshot
A mechanistic theory of hydrogen embrittlement of steels
inferredcites →https://doi.org/10.1007/978-1-4615-8258-8_2openalex-snapshot
Stress-Corrosion Cracking of Titanium Alloys
inferredcites →https://doi.org/10.1007/978-1-4757-0181-4openalex-snapshot
The Nature and Behavior of Grain Boundaries
inferredcites →https://doi.org/10.1007/bf00049196openalex-snapshot
The kinetics of subcritical crack growth under sustained loading
inferredcites →https://doi.org/10.1007/bf02641960openalex-snapshot
A short-time diffusion correlation for hydrogen-induced crack growth kinetics
inferredcites →https://doi.org/10.1007/bf02643219openalex-snapshot
Gaseous hydrogen-induced cracking of Ti-5Al-2.5Sn
inferredcites →https://doi.org/10.1007/bf02644334openalex-snapshot
Hydrogen transport through annealed and deformed armco iron
inferredcites →https://doi.org/10.1007/bf02644462openalex-snapshot
Hydrogen enhanced crack growth in 18 Ni maraging steels
inferredcites →https://doi.org/10.1007/bf02652858openalex-snapshot
The effect of reverted austenite on the mechanical properties and toughness of 12 Ni and 18 Ni (200) maraging steels
inferredcites →https://doi.org/10.1007/bf02664224openalex-snapshot
Embrittlement of a ferrous alloy in a partially dissociated hydrogen environment
inferredcites →https://doi.org/10.1007/bf02811638openalex-snapshot
The effective area concept, permeation, and hydrogen gas crack growth kinetics
inferredcites →https://doi.org/10.1007/bf02819243openalex-snapshot
Embrittlement of 4130 steel by low-pressure gaseous hydrogen
inferredcites →https://doi.org/10.1007/bf03038392openalex-snapshot
Embrittlement of titanium by liquid cadmium
inferredcites →https://doi.org/10.1016/0001-6160(70)90078-7openalex-snapshot
The diffusion and trapping of hydrogen in steel
inferredcites →https://doi.org/10.1016/0013-7944(68)90014-3openalex-snapshot
Sub-critical flaw growth
inferredcites →https://doi.org/10.1016/0013-7944(71)90039-7openalex-snapshot
A note on stress corrosion cracking rates
inferredcites →https://doi.org/10.1016/0013-7944(71)90047-6openalex-snapshot
Stress corrosion crack branching in high-strength steels
inferredcites →https://doi.org/10.1016/0036-9748(68)90222-6openalex-snapshot
Two-dimensional phase transformation in grain boundaries
inferredcites →https://doi.org/10.1016/0036-9748(72)90104-4openalex-snapshot
Slow crack growth in hydrogen and hydrogen sulfide gas environments
inferredcites →https://doi.org/10.1016/0036-9748(74)90017-9openalex-snapshot
Gaseous hydrogen assisted crack growth in 18 nickel maraging steels
inferredcites →https://doi.org/10.1016/0036-9748(74)90246-4openalex-snapshot
The effect of thickness on hydrogen-induced slow crack growth
inferredcites →https://doi.org/10.1016/0036-9748(76)90138-1openalex-snapshot
A technique for determining the elemental composition of fracture surfaces produced by crack growth in hydrogen and in water vapor
inferredcites →https://doi.org/10.1016/s0010-938x(65)80002-6openalex-snapshot
A study of the stress factor in corrosion cracking by use of the pre-cracked cantilever beam specimen
inferredcites →https://doi.org/10.1016/s0026-0576(01)81764-5openalex-snapshot
Hydrogen embrittlement testing
inferredcites →https://doi.org/10.1088/0031-9112/21/8/025openalex-snapshot
L'Hydrogène dans les Métaux
inferredcites →https://doi.org/10.1098/rspa.1953.0078openalex-snapshot
The kinetics of chemisorption of hydrogen and carbon monoxide on evaporated iron films
inferredcites →https://doi.org/10.1098/rspa.1953.0079openalex-snapshot
The sorption of hydrogen and other gases by evaporated iron films
inferredcites →https://doi.org/10.1111/j.1151-2916.1967.tb15145.xopenalex-snapshot
Influence of Water Vapor on Crack Propagation in Soda‐Lime Glass
inferredcites →https://doi.org/10.1115/1.3443102openalex-snapshot
Kinetics of Subcritical Crack Growth and Deformation in a High Strength Steel
inferredcites →https://doi.org/10.1116/1.1492421openalex-snapshot
Cryosorption Pumping of Hydrogen and Helium at 20 °K
inferredcites →https://doi.org/10.1520/jte10015jopenalex-snapshot
A Simple Method for Studying Slow Crack Growth
inferredcites →https://doi.org/10.1520/stp26584sopenalex-snapshot
Stress Analysis of Cracks
inferredcites →https://doi.org/10.1520/stp38937sopenalex-snapshot
Testing to Determine the Effect of High-Pressure Hydrogen Environments on the Mechanical Properties of Metals
inferredcites →https://doi.org/10.1520/stp38939sopenalex-snapshot
Disk Pressure Testing of Hydrogen Environment Embrittlement
inferredcites →https://doi.org/10.1520/stp44663sopenalex-snapshot
Plane Strain Crack Toughness Testing of High Strength Metallic Materials
inferredcites →https://doi.org/10.5006/0010-9312-24.10.313openalex-snapshot
Techniques for Investigating Hydrogen-Induced Cracking of Steels With High Yield Strength
inferredcites →https://doi.org/10.5006/0010-9312-29.8.299openalex-snapshot
Influence of Preloading on the Sustained Load Cracking Behavior of Maraging Steels in Hydrogen
inferredcites →https://doi.org/10.5006/0010-9312-31.2.42openalex-snapshot
Plateau Velocity of SCC in High Strength Steel — A Quantitative Treatment

What points at this work

Incoming claims: where this work appears in other papers’ reference lists and arguments.

inferred← citeshttps://doi.org/10.2139/ssrn.4092645openalex-extracted
inferred← citeshttps://doi.org/10.1002/9781118013373.ch12openalex-snapshot
The High Cycle Fatigue and Final Fracture Behavior of an Alloy Steel Used in Hydrogen Pressure Vessels: Influence of Notch
inferred← citeshttps://doi.org/10.1002/9781118788295.ch43openalex-snapshot
Transitions and Phase Equilibria among Grain Boundary Structures
inferred← citeshttps://doi.org/10.1002/9781118803363.ch85openalex-snapshot
Temperature Effects on Hydrogen‐Induced Cracking in an Iron‐Based Superalloy
inferred← citeshttps://doi.org/10.1002/9783527603978.mst0059openalex-snapshot
Fracture Mechanisms
inferred← citeshttps://doi.org/10.1002/maco.19820330102openalex-snapshot
Hydrogen embrittlement of construction materials
inferred← citeshttps://doi.org/10.1007/978-1-4613-3500-9_2openalex-snapshot
General Overview: Atomistics of Surface Reactions
inferred← citeshttps://doi.org/10.1007/978-1-4684-4130-7_5openalex-snapshot
The Chemistry of Gaseous Hydrogen Embrittlement
inferred← citeshttps://doi.org/10.1007/978-1-4899-1733-1_6openalex-snapshot
Environmental Cracking Of Metals
inferred← citeshttps://doi.org/10.1007/978-3-031-51350-3_18openalex-snapshot
Hydrogen Embrittlement and Sensitization Cracking
inferred← citeshttps://doi.org/10.1007/978-3-031-51350-3_19openalex-snapshot
Fracture Mechanics Approach to Stress Corrosion
inferred← citeshttps://doi.org/10.1007/978-88-470-2336-9_14openalex-snapshot
Hydrogen Embrittlement and Sensitization Cracking
inferred← citeshttps://doi.org/10.1007/978-88-470-2336-9_15openalex-snapshot
Fracture Mechanics Approach to Stress Corrosion
inferred← citeshttps://doi.org/10.1007/978-94-007-4930-6_7openalex-snapshot
Environment Assisted Cracking
inferred← citeshttps://doi.org/10.1007/978-94-011-1586-5_5openalex-snapshot
Thermoplastic Matrix Precursors
inferred← citeshttps://doi.org/10.1007/978-981-10-0161-1_6openalex-snapshot
Manifestations of Hydrogen Embrittlement
inferred← citeshttps://doi.org/10.1007/978-981-99-0992-6_6openalex-snapshot
Macroscopic Manifestations of Hydrogen Embrittlement
inferred← citeshttps://doi.org/10.1007/bf00465578openalex-snapshot
Temperature effects on gaseous hydrogen embrittlement of a high-strength steel
inferred← citeshttps://doi.org/10.1007/bf00610642openalex-snapshot
Kinetic aspects of slow crack growth in the gaseous hydrogen embrittlement of steels
inferred← citeshttps://doi.org/10.1007/bf00723075openalex-snapshot
The applicability of criteria of fracture mechanics for evaluating the hydrogen embrittlement of high-strength steels
inferred← citeshttps://doi.org/10.1007/bf00723304openalex-snapshot
Crack growth in deformed metals under the action of hydrogen
inferred← citeshttps://doi.org/10.1007/bf00728929openalex-snapshot
Measurement of the hydrogen brittleness of structural materials
inferred← citeshttps://doi.org/10.1007/bf02643402openalex-snapshot
The Effect of Stress State on Internal Hydrogen-Induced Crack Growth in Ti-6AI-6V-2Sn
inferred← citeshttps://doi.org/10.1007/bf02643688openalex-snapshot
Oxide-Induced Crack Closure: An Explanation for Near-Threshold Corrosion Fatigue Crack Growth Behavior
inferred← citeshttps://doi.org/10.1007/bf02643865openalex-snapshot
A comparative study of the embrittlement of monel 400 at room temperature by hydrogen and by mercury
inferred← citeshttps://doi.org/10.1007/bf02644205openalex-snapshot
Crack paths and hydrogen-Afinssisted crack growth response in AlSi 4340 steel
inferred← citeshttps://doi.org/10.1007/bf02644216openalex-snapshot
Kinetic enrichment of hydrogen at interfaces and voids by dislocation sweep-in of hydrogen
inferred← citeshttps://doi.org/10.1007/bf02646229openalex-snapshot
Comparison of hydrogen gas embrittlement of austenitic and ferritic stainless steels
inferred← citeshttps://doi.org/10.1007/bf02648345openalex-snapshot
Rate controlling processes for crack growth in hydrogen sulfide for an alsl 4340 steel
inferred← citeshttps://doi.org/10.1007/bf02648407openalex-snapshot
A strain-based fracture model for stress corrosion cracking of low-alloy steels
inferred← citeshttps://doi.org/10.1007/bf02651657openalex-snapshot
Microstructural trapping effects on hydrogen induced cracking of a microalloyed steel
inferred← citeshttps://doi.org/10.1007/bf02652220openalex-snapshot
Fracture mechanics and surface chemistry studies of subcritical crack growth in AISI 4340 steel
inferred← citeshttps://doi.org/10.1007/bf02654401openalex-snapshot
Hydrogen pressure dependence of the fracture mode transition in nickel
inferred← citeshttps://doi.org/10.1007/bf02654711openalex-snapshot
Hydrogen-induced slow crack growth in Ti-6Al-6V-2Sn
inferred← citeshttps://doi.org/10.1007/bf02661209openalex-snapshot
An adsorption study of hydrogen on iron and its relation to hydrogen embrittlement
inferred← citeshttps://doi.org/10.1007/bf02662405openalex-snapshot
A “Hydrogen partitioning” model for hydrogen assisted crack growth
inferred← citeshttps://doi.org/10.1007/bf02662593openalex-snapshot
Crack growth from internal hydrogen—temperature and microstructural effects in 4340 steel
inferred← citeshttps://doi.org/10.1007/bf02665007openalex-snapshot
A critical evaluation of the stress-corrosion cracking mechanism in high-strength aluminum alloys
inferred← citeshttps://doi.org/10.1007/bf02674033openalex-snapshot
Clean steels for steam turbine rotors—their stress corrosion cracking resistance
inferred← citeshttps://doi.org/10.1007/bf02697071openalex-snapshot
Effect of hydrogen on fracture of U-notched bend specimens of quenched and tempered AISI 4340 steel
inferred← citeshttps://doi.org/10.1007/bf02706442openalex-snapshot
Hydrogen embrittlement in power plant steels
inferred← citeshttps://doi.org/10.1007/bf03027481openalex-snapshot
Driving force for delayed Hydride cracking of zirconium alloys
inferred← citeshttps://doi.org/10.1007/bf03350949openalex-snapshot
The kinetics and micromechanics of hydrogen assisted cracking in Fe-3 pct Si single crystals
inferred← citeshttps://doi.org/10.1007/bf03350963openalex-snapshot
Hydrogen compatibility of Femnal alloys
inferred← citeshttps://doi.org/10.1007/bfb0103404openalex-snapshot
Hydrogen related material problems
inferred← citeshttps://doi.org/10.1007/s11090-022-10268-wopenalex-snapshot
Dielectric Barrier Discharge Plasma Deoxidation of Copper Surfaces in an Ar/SiH4 Atmosphere
inferred← citeshttps://doi.org/10.1007/s11661-003-0334-3openalex-snapshot
Internal hydrogen embrittlement of ultrahigh-strength AERMET 100 steel
inferred← citeshttps://doi.org/10.1007/s11661-012-1133-5openalex-snapshot
Fatigue Crack Growth under High Pressure of Gaseous Hydrogen in a 15-5PH Martensitic Stainless Steel: Influence of Pressure and Loading Frequency
inferred← citeshttps://doi.org/10.1007/s11661-012-1359-2openalex-snapshot
Mechanisms and Kinetics of Environmentally Assisted Cracking: Current Status, Issues, and Suggestions for Further Work
inferred← citeshttps://doi.org/10.1007/s11661-012-1403-2openalex-snapshot
Studies of Evaluation of Hydrogen Embrittlement Property of High-Strength Steels with Consideration of the Effect of Atmospheric Corrosion
inferred← citeshttps://doi.org/10.1007/s11665-997-0011-6openalex-snapshot
Hydrogen embrittlement of a Ti-strengthened 250 grade maraging steel
inferred← citeshttps://doi.org/10.1007/s11837-021-04667-1openalex-snapshot
Griffith’s Legacy to Alloy Design and Beyond
inferred← citeshttps://doi.org/10.1016/0001-6160(83)90044-5openalex-snapshot
A work function-chemisorption study of hydrogen on iron: Kinetics and strain effects
inferred← citeshttps://doi.org/10.1016/0001-6160(83)90125-6openalex-snapshot
Gaseous hydrogen embrittlement in FeSi- and Ni-single crystals
inferred← citeshttps://doi.org/10.1016/0001-6160(85)90189-0openalex-snapshot
Hydrogen embrittlement and trapping at crack tips in Ni-single crystals
inferred← citeshttps://doi.org/10.1016/0001-6160(87)90111-8openalex-snapshot
A Comparison of hydrogen and mercury embrittlement in aisi 4142 steel
inferred← citeshttps://doi.org/10.1016/0001-6160(88)90277-5openalex-snapshot
Effects of water vapor and hydrogen sulfide on hydrogen permeation in stainless steels
inferred← citeshttps://doi.org/10.1016/0001-6160(89)90286-1openalex-snapshot
Deuterium concentration profiles in FeNiCo alloys electrochemically charged at room temperature
inferred← citeshttps://doi.org/10.1016/0010-938x(80)90060-8openalex-snapshot
Comparison of fracture test data for some high strength steels stressed in a saline medium and in gaseous hydrogen
inferred← citeshttps://doi.org/10.1016/0022-3115(83)90072-7openalex-snapshot
Chemical aspects of iodine-induced stress corrosion cracking failure of zircaloy-4 tubing above 50°C
inferred← citeshttps://doi.org/10.1016/0036-9748(76)90138-1openalex-snapshot
A technique for determining the elemental composition of fracture surfaces produced by crack growth in hydrogen and in water vapor
inferred← citeshttps://doi.org/10.1016/0036-9748(78)90021-2openalex-snapshot
A preliminary investigation of hart's model in hydrogen embrittlement in maraging steels
inferred← citeshttps://doi.org/10.1016/0036-9748(81)90246-5openalex-snapshot
Gaseous hydrogen embrittlement of steel — The rate controlling process
inferred← citeshttps://doi.org/10.1016/0036-9748(81)90262-3openalex-snapshot
The rate controlling step in stage II crack growth rates during gaseous hydrogen embrittlement
inferred← citeshttps://doi.org/10.1016/0036-9748(82)90249-6openalex-snapshot
A surface chemistry kinetic model of gaseous hydrogen embrittlement
inferred← citeshttps://doi.org/10.1016/0036-9748(86)90485-0openalex-snapshot
Temperature effects on hydrogen assisted crack growth in internally charged AISI 4340 steel
inferred← citeshttps://doi.org/10.1016/0956-7151(92)90192-hopenalex-snapshot
Temperature effects on the mechanism of time independent hydrogen assisted fatigue crack propagation in steels
inferred← citeshttps://doi.org/10.1016/0956-7151(92)90347-hopenalex-snapshot
The application of surface science to fatigue: The role of surface chemistry and surface modification in fatigue crack initiation in silver single crystals
inferred← citeshttps://doi.org/10.1016/1359-6454(95)00429-7openalex-snapshot
Hydrogen-assisted stable crack growth in iron-3 wt% silicon steel
inferred← citeshttps://doi.org/10.1016/b0-08-043749-4/06134-6openalex-snapshot
Hydrogen-assisted Cracking
inferred← citeshttps://doi.org/10.1016/b978-0-08-034813-1.50025-5openalex-snapshot
A WORK FUNCTION-CHEMISORPTION STUDY OF HYDROGEN ON IRON: KINETICS AND STRAIN EFFECTS
inferred← citeshttps://doi.org/10.1016/b978-0-08-034813-1.50091-7openalex-snapshot
GASEOUS HYDROGEN EMBRITTLEMENT IN FeSi- AND Ni-SINGLE CRYSTALS
inferred← citeshttps://doi.org/10.1016/b978-0-08-034813-1.50092-9openalex-snapshot
HYDROGEN EMBRITTLEMENT AND TRAPPING AT CRACK TIPS IN Ni-SINGLE CRYSTALS
inferred← citeshttps://doi.org/10.1016/b978-012709120-4/50007-3openalex-snapshot
References
inferred← citeshttps://doi.org/10.1016/b978-044452787-5.00038-xopenalex-snapshot
Corrosion Fatigue*
inferred← citeshttps://doi.org/10.1016/b978-1-4832-8414-9.50075-4openalex-snapshot
THE TEMPERATURE DEPENDENCE OF THRESHOLDS IN AN α/β TITANIUM ALLOY
inferred← citeshttps://doi.org/10.1016/j.actamat.2019.04.040openalex-snapshot
Effects of lamellar structure on tensile properties and resistance to hydrogen embrittlement of pearlitic steel
inferred← citeshttps://doi.org/10.1016/j.actamat.2021.117567openalex-snapshot
Micro-axial cracking in unnotched, cold-drawn pearlitic steel wire: Mechanism and beneficial effect on the resistance to hydrogen embrittlement
inferred← citeshttps://doi.org/10.1016/j.corsci.2011.09.008openalex-snapshot
Hydrogen trapping in an API 5L X60 steel
inferred← citeshttps://doi.org/10.1016/j.corsci.2023.111163openalex-snapshot
Investigation of quasi-cleavage in a hydrogen charged maraging stainless steel
inferred← citeshttps://doi.org/10.1016/j.electacta.2020.137422openalex-snapshot
Quantitative calibration of the relationship between Volta potential measured by scanning Kelvin probe force microscope (SKPFM) and hydrogen concentration
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2025.109885openalex-snapshot
Effect of water temperature in the deep sea on the mitigation of hydrogen embrittlement by O2 impurity
inferred← citeshttps://doi.org/10.1016/j.engfracmech.2015.12.002openalex-snapshot
About the fatigue crack propagation threshold of metals as a design criterion – A review
inferred← citeshttps://doi.org/10.1016/j.engfracmech.2019.106502openalex-snapshot
The role of atomistic simulations in probing hydrogen effects on plasticity and embrittlement in metals
inferred← citeshttps://doi.org/10.1016/j.ijfatigue.2005.04.011openalex-snapshot
Evaluation of environmental effects on fatigue crack growth behaviour of a high strength steel in a saline solution with cathodic protection
inferred← citeshttps://doi.org/10.1016/j.ijfatigue.2013.04.018openalex-snapshot
Influence of dissolved hydrogen on the fatigue crack growth behaviour of AISI 4140 steel
inferred← citeshttps://doi.org/10.1016/j.ijfatigue.2013.08.010openalex-snapshot
Modeling the fatigue crack growth of X100 pipeline steel in gaseous hydrogen
inferred← citeshttps://doi.org/10.1016/j.ijfatigue.2015.06.002openalex-snapshot
Fatigue behavior of hydrogen pre-charged low alloy Cr–Mo steel
inferred← citeshttps://doi.org/10.1016/j.ijfatigue.2017.06.030openalex-snapshot
Interdisciplinary multi-scale research on environment assisted cracking: The 50 year legacy of Robert P. Wei
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2021.07.136openalex-snapshot
Hydrogen embrittlement and associated surface crack growth in fine-grained equiatomic CoCrFeMnNi high-entropy alloys with different annealing temperatures evaluated by tensile testing under in situ hydrogen charging
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2024.01.232openalex-snapshot
Hydrogen embrittlement and hydrogen-induced crack initiation in additively manufactured metals: A critical review on mechanical and cyclic loading
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2024.05.257openalex-snapshot
Review of the hydrogen embrittlement and interactions between hydrogen and microstructural interfaces in metallic alloys: Grain boundary, twin boundary, and nano-precipitate
inferred← citeshttps://doi.org/10.1016/j.jcsr.2024.108840openalex-snapshot
Mechanical performance of high strength steel under corrosion: A review study
inferred← citeshttps://doi.org/10.1016/j.jsse.2023.05.002openalex-snapshot
A critical review on very high cycle corrosion fatigue: Mechanisms, methods, materials, and models
inferred← citeshttps://doi.org/10.1016/j.mechrescom.2018.03.003openalex-snapshot
Fracture mechanics – An interpretive technical history
inferred← citeshttps://doi.org/10.1016/j.msea.2017.07.019openalex-snapshot
The effect of heat-to-heat variations in metallurgy and hydrogen-metal interactions on the hydrogen embrittlement of Monel K-500
inferred← citeshttps://doi.org/10.1016/j.msea.2022.143394openalex-snapshot
Hydrogen-Accelerated Fatigue Crack Growth of Equiatomic Fe–Cr–Ni–Mn–Co High-Entropy Alloy Evaluated by Compact Tension Testing
inferred← citeshttps://doi.org/10.1016/j.proeng.2015.06.211openalex-snapshot
Technique for Improving Paris-Erdogan Constants of Steels in Hydrogen Environment
inferred← citeshttps://doi.org/10.1016/j.tafmec.2015.11.003openalex-snapshot
Simulation of hydrogen assisted-cracking in terms of its growth phenomenon
inferred← citeshttps://doi.org/10.1016/s0013-7944(00)00122-3openalex-snapshot
Temperature effects on hydrogen-induced crack growth susceptibility of iron-based superalloys
inferred← citeshttps://doi.org/10.1016/s0026-0657(10)80057-8openalex-snapshot
Production and densification of carbon-carbon composites using HIP techniques
inferred← citeshttps://doi.org/10.1016/s0142-1123(02)00002-6openalex-snapshot
Mapping of the rate-controlling steps for environment-assisted fatigue crack growth applied to the aluminium alloy 6013 T6
inferred← citeshttps://doi.org/10.1017/cbo9780511806865openalex-snapshot
Fracture Mechanics
inferred← citeshttps://doi.org/10.1017/cbo9780511806865.009openalex-snapshot
Subcritical Crack Growth: Environmentally Enhanced Crack Growth under Sustained Loads (or Stress Corrosion Cracking)
inferred← citeshttps://doi.org/10.1017/cbo9780511806865.012openalex-snapshot
APPENDIX: Publications by R. P. Wei and Colleagues
inferred← citeshttps://doi.org/10.1039/d5cp02423dopenalex-snapshot
Kinetic modeling of ammonia and hydrogen dissociative co-adsorption on iron surface and its effect on hydrogen embrittlement
inferred← citeshttps://doi.org/10.1080/01418619108204854openalex-snapshot
The necessity of both plasticity and brittleness in the fracture thresholds of iron
inferred← citeshttps://doi.org/10.1088/1361-651x/ab84c2openalex-snapshot
Solute segregation to near-coincidence site lattice grain boundaries in α-iron
inferred← citeshttps://doi.org/10.1103/physrevlett.116.075502openalex-snapshot
Chemomechanical Origin of Hydrogen Trapping at Grain Boundaries in fcc Metals
inferred← citeshttps://doi.org/10.1111/ffe.12994openalex-snapshot
Inhibitory effect of oxygen on hydrogen‐induced fracture of A333 pipe steel
inferred← citeshttps://doi.org/10.1111/j.1460-2695.1981.tb01372.xopenalex-snapshot
ELECTRICAL POTENTIAL MONITORING OF CRACK FORMATION AND SUBCRITICAL GROWTH FROM SMALL DEFECTS
inferred← citeshttps://doi.org/10.1111/j.1460-2695.1997.tb00304.xopenalex-snapshot
K‐DOMINANCE CONDITION IN HYDROGEN ASSISTED CRACKING: THE ROLE OF THE FAR FIELD
inferred← citeshttps://doi.org/10.1111/j.1460-2695.1997.tb01545.xopenalex-snapshot
ASSISTED CRACK GROWTH IN MARAGING STEEL WELDS BY GASEOUS HYDROGEN
inferred← citeshttps://doi.org/10.1111/j.1460-2695.2010.01526.xopenalex-snapshot
Influence of activation energy and sensitivity to hydrogen embrittlement on fatigue strength degradation by irreversible hydrogen in high-strength steels
inferred← citeshttps://doi.org/10.1115/1.3224813openalex-snapshot
Near-Threshold Fatigue Crack Growth in 2 1/4 Cr-1Mo Pressure Vessel Steel in Air and Hydrogen
inferred← citeshttps://doi.org/10.1179/026708389790222672openalex-snapshot
Crack propagation of secondary hardened alloy steels in gaseous hydrogen atmosphere
inferred← citeshttps://doi.org/10.1179/imtr.1978.23.1.164openalex-snapshot
Intergranularfailure in steel: the role of grain-boundary composition
inferred← citeshttps://doi.org/10.1179/imtr.1979.24.1.205openalex-snapshot
Near-threshold fatigue-crack propagation in steels
inferred← citeshttps://doi.org/10.1179/msc.1979.13.7.429openalex-snapshot
Effect of aqueous and hydrogen environments on fatigue crack growth in 2Ni-Cr-Mo-V rotor steel
inferred← citeshttps://doi.org/10.1299/kikaia.76.1204openalex-snapshot
Effects of Hydrogen Concentration, Specimen Thickness, Loading Frequency and Temperature on the Hydrogen Enhanced Crack Propagation of Low Alloy Steel
inferred← citeshttps://doi.org/10.14393/ufu.te.2021.5554openalex-snapshot
Efeito de parâmetros microestruturais e da temperatura do meio na susceptibilidade à fragilização por hidrogênio de aços de alta resistência e baixa liga
inferred← citeshttps://doi.org/10.1515/corrrev-2015-0034openalex-snapshot
Crack growth behavior of 4340 steel under corrosion and corrosion fatigue conditions
inferred← citeshttps://doi.org/10.1515/corrrev-2016-0006openalex-snapshot
A review of hydrogen embrittlement of martensitic advanced high-strength steels
inferred← citeshttps://doi.org/10.1520/stp15067sopenalex-snapshot
Direct Current Electrical Potential Measurement of the Growth of Small Cracks
inferred← citeshttps://doi.org/10.1520/stp18827sopenalex-snapshot
Environmentally Assisted Crack Growth in Structural Alloys: Perspectives and New Directions
inferred← citeshttps://doi.org/10.1520/stp33456sopenalex-snapshot
An Assessment of A-C and D-C Potential Systems for Monitoring Fatigue Crack Growth
inferred← citeshttps://doi.org/10.1520/stp38087sopenalex-snapshot
Fractographic Analysis of Gaseous Hydrogen Induced Cracking in 18Ni Maraging Steel
inferred← citeshttps://doi.org/10.1533/9780857093769.1.90openalex-snapshot
Hydrogen embrittlement (HE) phenomena and mechanisms
inferred← citeshttps://doi.org/10.1533/9780857093899.2.195openalex-snapshot
Fracture and fatigue test methods in hydrogen gas
inferred← citeshttps://doi.org/10.1533/9780857093899.3.421openalex-snapshot
Hydrogen embrittlement of high strength steels
inferred← citeshttps://doi.org/10.1533/9780857095374.1.89openalex-snapshot
Hydrogen diffusion and trapping in metals
inferred← citeshttps://doi.org/10.1533/9780857095374.2.209openalex-snapshot
Modeling hydrogen induced damage mechanisms in metals
inferred← citeshttps://doi.org/10.1533/9780857095374.2.430openalex-snapshot
Development of service life prognosis systems for hydrogen energy devices
inferred← citeshttps://doi.org/10.18130/v3zc62openalex-snapshot
Local Probe Techniques for Hydrogen Measurement in Ultra-High Strength Steels
inferred← citeshttps://doi.org/10.2172/993303openalex-snapshot
Measurement and interpretation of threshold stress intensity factors for steels in high-pressure hydrogen gas.
inferred← citeshttps://doi.org/10.2320/matertrans1960.28.957openalex-snapshot
Crack Propagation of High Strength Steels in Oxygen-doped Hydrogen Gas
inferred← citeshttps://doi.org/10.2320/matertrans1989.35.879openalex-snapshot
Critical Pressures of Water Vapor and Hydrogen Gas Causing Intergranular Brittle Fracture of Co3Ti at Room Temperature
inferred← citeshttps://doi.org/10.2355/isijinternational.52.307openalex-snapshot
Evaluation of Delayed Fracture Property of High Strength Bolt Steels
inferred← citeshttps://doi.org/10.2472/jsms.60.898openalex-snapshot
Effect of Heat Treatment on the Hydrogen Enhanced Fatigue Crack Propagation of Low Carbon Steel S25C
inferred← citeshttps://doi.org/10.29027/ijirase.v2.i6.2018.302-308openalex-snapshot
Experimental Investigation of Hydrogen Embrittlement in Industrial Steels
inferred← citeshttps://doi.org/10.31399/asm.ash.cas.t66110452openalex-snapshot
Stress-Corrosion Cracking of Steels
inferred← citeshttps://doi.org/10.31399/asm.ash.cas.t66110477openalex-snapshot
Hydrogen Damage of Steels
inferred← citeshttps://doi.org/10.31399/asm.hb.v01.a0001039openalex-snapshot
Embrittlement of Steels
inferred← citeshttps://doi.org/10.31399/asm.hb.v19.a0002361openalex-snapshot
Mechanisms of Corrosion Fatigue
inferred← citeshttps://doi.org/10.31399/asm.tb.sccmpe2.t55090067openalex-snapshot
Stress-Corrosion Cracking of High-Strength Steels (Yield Strengths Greater Than 1240 MPa)
inferred← citeshttps://doi.org/10.3221/igf-esis.35.30openalex-snapshot
A cohesive zone model to simulate the hydrogen embrittlement effect on a high-strength steel
inferred← citeshttps://doi.org/10.3323/jcorr.60.184openalex-snapshot
Delayed Fracture of High Strength Steels under Atmospheric Corrosion
inferred← citeshttps://doi.org/10.3390/met11030423openalex-snapshot
Review on the Influence of Temperature upon Hydrogen Effects in Structural Alloys
inferred← citeshttps://doi.org/10.3390/nano11020294openalex-snapshot
The Role of Hydrogen on the Behavior of Intergranular Cracks in Bicrystalline α-Fe Nanowires
inferred← citeshttps://doi.org/10.3740/mrsk.2011.21.11.581openalex-snapshot
Hydrogen Embrittlement Evaluation of Subsurface Zone in 590DP Steel by Micro-Vickers Hardness Measurement
inferred← citeshttps://doi.org/10.5006/1.3583875openalex-snapshot
Whitney Award Lecture—1987: Hydrogen—The Versatile Embrittler
inferred← citeshttps://doi.org/10.5006/1.3584950openalex-snapshot
Effect of Temperature and Ionic Impurities at Very Low Concentrations on Stress Corrosion Cracking of AISI 304 Stainless Steel
inferred← citeshttps://doi.org/10.5006/1.3585134openalex-snapshot
Stress Corrosion Cracking of High-Strength Steels in Aqueous Environments
inferred← citeshttps://doi.org/10.5006/3240openalex-snapshot
Hydrogen Embrittlement of Low Alloy Steels Under Cathodic Polarization
inferred← citeshttps://doi.org/10.5006/c1985-85102openalex-snapshot
Effect of Temperature and Ionic Impurities at Very Low Concentrations on Stress Corrosion Cracking of Type 304 Stainless Steel
inferred← citeshttps://doi.org/10.5006/c2007-07493openalex-snapshot
Progress towards Understanding Mechanisms of Hydrogen Embrittlement and Stress Corrosion Cracking
inferred← citeshttps://doi.org/10.6028/jres.119.002openalex-snapshot
Sensitivity Analysis of Fatigue Crack Growth Model for API Steels in Gaseous Hydrogen
inferred← citeshttps://doi.org/10.6028/jres.124.008openalex-snapshot
Fatigue Testing of Pipeline Welds and Heat-Affected Zones in Pressurized Hydrogen Gas
inferred← citeshttps://doi.org/10.7939/r3j679788openalex-snapshot
Crack Growth Behavior of Pipeline Steels under Variable Pressure Fluctuations in a Near-Neutral pH Environment
Editorial review for independent work. ICSAC — the Institute for Complexity Science and Advanced Computing — runs a structured editorial panel for researchers publishing outside journals, and publishes on CiteStamp rails. Submission is free and goes through ORCID: icsacinstitute.org/submit.