On the public citation graph

Microstructure design strategies to mitigate hydrogen embrittlement in metallic materials

0 signed · 173 inferred · view as graph

Inferred edges come from two machine sources: sweeps of open repository metadata (mostly SSRN and Zenodo), and a bulk OpenAlex citation snapshot. Every row below is labelled with the one it came from. Neither is a complete citation index — absence here is not evidence of absence.

Is this your work? Sign in with ORCID and put your name on the claims that are yours.
Claim with ORCID
Reference health. See whether every reference in this work resolves to a known work and none has been retracted — and get a dated CiteStamped badge you can embed.
See reference health

What this work says

Outgoing claims: the papers this work cites, builds on, or argues with.

inferredcites →https://doi.org/10.1002/bbpc.19720760864openalex-snapshot
A mechanistic theory of hydrogen embrittlement of steels
inferredcites →https://doi.org/10.1007/bf00540409openalex-snapshot
Hydrogen trapping phenomena in carbon steel
inferredcites →https://doi.org/10.1007/bf02642048openalex-snapshot
A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)
inferredcites →https://doi.org/10.1007/bf02642424openalex-snapshot
Thermal analysis of trapped hydrogen in pure iron
inferredcites →https://doi.org/10.1007/bf02646139openalex-snapshot
Evaluation of hydrogen-trap binding enthalpy l
inferredcites →https://doi.org/10.1007/bf02661939openalex-snapshot
A quantitative analysis of hydrogen trapping
inferredcites →https://doi.org/10.1007/bf02663432openalex-snapshot
Hydrogen transport in nickel-base alloys
inferredcites →https://doi.org/10.1007/s10853-012-6526-8openalex-snapshot
Impact of heat treatment on the mechanical properties of AISI 304L austenitic stainless steel in high-pressure hydrogen gas
inferredcites →https://doi.org/10.1007/s11661-000-0064-8openalex-snapshot
The identification of hydrogen trapping states in an Al-Li-Cu-Zr alloy using thermal desorption spectroscopy
inferredcites →https://doi.org/10.1007/s11661-001-0268-6openalex-snapshot
The effect of strain on the trapping of hydrogen at grain-boundary carbides in Ni-Cr-Fe alloys
inferredcites →https://doi.org/10.1007/s11661-004-0060-5openalex-snapshot
Hydrogen absorption of incoherent TiC particles in iron from environment at high temperatures
inferredcites →https://doi.org/10.1007/s11661-006-0004-3openalex-snapshot
Quantitative analysis on hydrogen trapping of TiC particles in steel
inferredcites →https://doi.org/10.1007/s11661-010-0558-yopenalex-snapshot
Effect of Hydrogen on Tensile Properties of Ultrafine-Grained Type 310S Austenitic Stainless Steel Processed by High-Pressure Torsion
inferredcites →https://doi.org/10.1007/s11661-013-2181-1openalex-snapshot
Thermal Desorption Spectroscopy Evaluation of the Hydrogen-Trapping Capacity of NbC and NbN Precipitates
inferredcites →https://doi.org/10.1007/s11661-020-05947-2openalex-snapshot
Current Challenges and Opportunities in Microstructure-Related Properties of Advanced High-Strength Steels
inferredcites →https://doi.org/10.1007/s11661-020-05966-zopenalex-snapshot
Effects of Mn Content and Grain Size on Hydrogen Embrittlement Susceptibility of Face-Centered Cubic High-Entropy Alloys
inferredcites →https://doi.org/10.1007/s11663-015-0325-yopenalex-snapshot
Hydrogen Embrittlement Understood
inferredcites →https://doi.org/10.1007/s40195-021-01233-1openalex-snapshot
Current Challenges and Opportunities Toward Understanding Hydrogen Embrittlement Mechanisms in Advanced High-Strength Steels: A Review
inferredcites →https://doi.org/10.1007/s40195-022-01483-7openalex-snapshot
Enhancing the Hydrogen Embrittlement Resistance of Medium Mn Steels by Designing Metastable Austenite with a Compositional Core–shell Structure
inferredcites →https://doi.org/10.1016/0001-6160(80)90112-1openalex-snapshot
Adsorption-induced interface decohesion
inferredcites →https://doi.org/10.1016/0001-6160(84)90210-4openalex-snapshot
Hydrogen trapping by TiC particles in iron
inferredcites →https://doi.org/10.1016/0001-6160(88)90113-7openalex-snapshot
Environmentally assisted cracking: Overview of evidence for an adsorption-induced localised-slip process
inferredcites →https://doi.org/10.1016/0001-6160(89)90286-1openalex-snapshot
Deuterium concentration profiles in FeNiCo alloys electrochemically charged at room temperature
inferredcites →https://doi.org/10.1016/0025-5416(85)90080-1openalex-snapshot
Effects of Fe3C and Mo2C precipitation on hydrogen diffusivity and hydrogen embrittlement in iron alloys
inferredcites →https://doi.org/10.1016/0026-0800(89)90016-5openalex-snapshot
Metallographic contributions to understanding mechanisms of environmentally assisted cracking
inferredcites →https://doi.org/10.1016/0036-9748(83)90242-9openalex-snapshot
The measurement of the trap binding energy by the thermal analysis technique
inferredcites →https://doi.org/10.1016/0921-5093(94)90975-xopenalex-snapshot
Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture
inferredcites →https://doi.org/10.1016/j.actamat.2009.05.012openalex-snapshot
Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials
inferredcites →https://doi.org/10.1016/j.actamat.2011.11.009openalex-snapshot
Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles
inferredcites →https://doi.org/10.1016/j.actamat.2012.01.040openalex-snapshot
Hydrogen-induced intergranular failure in nickel revisited
inferredcites →https://doi.org/10.1016/j.actamat.2012.04.010openalex-snapshot
Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel
inferredcites →https://doi.org/10.1016/j.actamat.2013.02.007openalex-snapshot
Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)
inferredcites →https://doi.org/10.1016/j.actamat.2014.01.048openalex-snapshot
Hydrogen-assisted decohesion and localized plasticity in dual-phase steel
inferredcites →https://doi.org/10.1016/j.actamat.2014.01.060openalex-snapshot
Hydrogen-induced intergranular failure of iron
inferredcites →https://doi.org/10.1016/j.actamat.2017.02.059openalex-snapshot
Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: The role of localized deformation in crack propagation
inferredcites →https://doi.org/10.1016/j.actamat.2018.05.003openalex-snapshot
Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel
inferredcites →https://doi.org/10.1016/j.actamat.2018.11.029openalex-snapshot
Revealing fracture mechanisms of medium manganese steels with and without delta-ferrite
inferredcites →https://doi.org/10.1016/j.actamat.2019.11.029openalex-snapshot
Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels
inferredcites →https://doi.org/10.1016/j.actamat.2020.06.051openalex-snapshot
Effects of Cu addition on resistance to hydrogen embrittlement in 1 GPa-grade duplex lightweight steels
inferredcites →https://doi.org/10.1016/j.actamat.2020.09.007openalex-snapshot
Phase boundary segregation-induced strengthening and discontinuous yielding in ultrafine-grained duplex medium-Mn steels
inferredcites →https://doi.org/10.1016/j.actamat.2020.09.031openalex-snapshot
Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces
inferredcites →https://doi.org/10.1016/j.actamat.2021.116661openalex-snapshot
Effects of solid solution and grain-boundary segregation of Mo on hydrogen embrittlement in 32MnB5 hot-stamping steels
inferredcites →https://doi.org/10.1016/j.actamat.2021.117488openalex-snapshot
Hydrogen embrittlement mechanisms in advanced high strength steel
inferredcites →https://doi.org/10.1016/j.actamat.2022.118296openalex-snapshot
Hydrogen-associated decohesion and localized plasticity in a high-Mn and high-Al two-phase lightweight steel
inferredcites →https://doi.org/10.1016/j.actamat.2022.118392openalex-snapshot
Hydrogen-assisted decohesion associated with nanosized grain boundary κ-carbides in a high-Mn lightweight steel
inferredcites →https://doi.org/10.1016/j.commatsci.2018.03.009openalex-snapshot
First-principles study of hydrogen segregation at the MgZn2 precipitate in Al-Mg-Zn alloys
inferredcites →https://doi.org/10.1016/j.corcom.2022.02.003openalex-snapshot
Tailoring hydrogen embrittlement resistance of pure Ni by grain boundary engineering
inferredcites →https://doi.org/10.1016/j.corsci.2005.11.004openalex-snapshot
Hydrogen uptake in 316L stainless steel: Consequences on the tensile properties
inferredcites →https://doi.org/10.1016/j.corsci.2014.08.005openalex-snapshot
The effect of Ti precipitates on hydrogen embrittlement of Fe–18Mn–0.6C–2Al–xTi twinning-induced plasticity steel
inferredcites →https://doi.org/10.1016/j.corsci.2015.01.012openalex-snapshot
The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel
inferredcites →https://doi.org/10.1016/j.corsci.2016.07.013openalex-snapshot
The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys
inferredcites →https://doi.org/10.1016/j.corsci.2018.07.028openalex-snapshot
Effect of grain boundary engineering on hydrogen embrittlement in Fe-Mn-C TWIP steel at various strain rates
inferredcites →https://doi.org/10.1016/j.corsci.2022.110331openalex-snapshot
Hydrogen assisted intergranular cracking of alloy 725: The effect of boron and copper alloying
inferredcites →https://doi.org/10.1016/j.cossms.2014.06.002openalex-snapshot
Grain boundary segregation engineering in metallic alloys: A pathway to the design of interfaces
inferredcites →https://doi.org/10.1016/j.engfailanal.2013.04.028openalex-snapshot
A comparative study of hydrogen induced cracking behavior in API 5L X60 and X70 pipeline steels
inferredcites →https://doi.org/10.1016/j.engfailanal.2015.05.017openalex-snapshot
Hydrogen damage of steels: A case study and hydrogen embrittlement model
inferredcites →https://doi.org/10.1016/j.engfracmech.2019.106528openalex-snapshot
The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion
inferredcites →https://doi.org/10.1016/j.ijhydene.2010.06.018openalex-snapshot
On the physical differences between tensile testing of type 304 and 316 austenitic stainless steels with internal hydrogen and in external hydrogen
inferredcites →https://doi.org/10.1016/j.ijhydene.2011.05.027openalex-snapshot
Hydrogen interaction with multiple traps: Can it be used to mitigate embrittlement?
inferredcites →https://doi.org/10.1016/j.ijhydene.2011.12.035openalex-snapshot
Suppression of hydrogen-assisted fatigue crack growth in austenitic stainless steel by cavitation peening
inferredcites →https://doi.org/10.1016/j.ijhydene.2012.08.071openalex-snapshot
Hydrogen environment embrittlement of stable austenitic steels
inferredcites →https://doi.org/10.1016/j.ijhydene.2013.12.171openalex-snapshot
Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe–Mn–Al–C light weight austenitic steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2015.06.111openalex-snapshot
Critical grain size to limit the hydrogen-induced ductility drop in a metastable austenitic steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2015.06.112openalex-snapshot
Effects of grain size on hydrogen embrittlement in a Fe-22Mn-0.6C TWIP steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2016.05.176openalex-snapshot
Evaluation of the role of Mo2C in hydrogen induced ductility loss in Q&T Fe C Mo alloys
inferredcites →https://doi.org/10.1016/j.ijhydene.2018.04.048openalex-snapshot
Grain boundary engineering approach to improve hydrogen embrittlement resistance in Fe Mn C TWIP steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2018.05.037openalex-snapshot
Strengthening mechanism and hydrogen-induced crack resistance of AISI 316L stainless steel subjected to laser peening at different power densities
inferredcites →https://doi.org/10.1016/j.ijhydene.2018.06.064openalex-snapshot
Hydrogen related degradation in pipeline steel: A review
inferredcites →https://doi.org/10.1016/j.ijhydene.2019.04.280openalex-snapshot
Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy
inferredcites →https://doi.org/10.1016/j.ijhydene.2019.05.074openalex-snapshot
The effect of prior austenite grain size on hydrogen embrittlement of Co-containing 18Ni 300 maraging steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2019.07.179openalex-snapshot
Relationship between hydrogen embrittlement and Md30 temperature: Prediction of low-nickel austenitic stainless steel's resistance
inferredcites →https://doi.org/10.1016/j.ijhydene.2019.11.102openalex-snapshot
Density functional theory calculations of iron - vanadium carbide interfaces and the effect of hydrogen
inferredcites →https://doi.org/10.1016/j.ijhydene.2020.01.021openalex-snapshot
Effect of shot peening coverage on hydrogen embrittlement of a ferrite-pearlite steel
inferredcites →https://doi.org/10.1016/j.ijhydene.2021.09.013openalex-snapshot
Influence of microstructure-driven hydrogen distribution on environmental hydrogen embrittlement of an Al–Cu–Mg alloy
inferredcites →https://doi.org/10.1016/j.ijhydene.2022.07.164openalex-snapshot
Permeation barriers for hydrogen embrittlement prevention in metals – A review on mechanisms, materials suitability and efficiency
inferredcites →https://doi.org/10.1016/j.jmps.2017.12.016openalex-snapshot
Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels
inferredcites →https://doi.org/10.1016/j.jmrt.2022.07.061openalex-snapshot
Hydrogen embrittlement micromechanisms and direct observations of hydrogen transportation by dislocations during deformation in a carbon-doped medium entropy alloy
inferredcites →https://doi.org/10.1016/j.jmst.2017.09.011openalex-snapshot
Hydrogen transport in metals: Integration of permeation, thermal desorption and degassing
inferredcites →https://doi.org/10.1016/j.jmst.2019.03.043openalex-snapshot
Effect of grain refinement on the hydrogen embrittlement of 304 austenitic stainless steel
inferredcites →https://doi.org/10.1016/j.jngse.2022.104709openalex-snapshot
Hydrogen in pipeline steels: Recent advances in characterization and embrittlement mitigation
inferredcites →https://doi.org/10.1016/j.matchar.2020.110386openalex-snapshot
The possibility of enhanced hydrogen embrittlement resistance of medium-Mn steels by addition of micro-alloying elements
inferredcites →https://doi.org/10.1016/j.matdes.2016.07.121openalex-snapshot
The dual role of shot peening in hydrogen-assisted cracking of PSB1080 high strength steel
inferredcites →https://doi.org/10.1016/j.msea.2003.12.096openalex-snapshot
The effect of copper precipitation on hydrogen embrittlement in iron
inferredcites →https://doi.org/10.1016/j.msea.2006.07.089openalex-snapshot
Interaction of hydrogen with the microstructure of low-carbon steel
inferredcites →https://doi.org/10.1016/j.msea.2015.11.017openalex-snapshot
Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel
inferredcites →https://doi.org/10.1016/j.msea.2016.02.003openalex-snapshot
Hydrogen isotope trapping in Al–Cu binary alloys
inferredcites →https://doi.org/10.1016/j.msea.2016.05.018openalex-snapshot
Hydrogen trapping and hydrogen induced mechanical degradation in lab cast Fe-C-Cr alloys
inferredcites →https://doi.org/10.1016/j.msea.2016.08.053openalex-snapshot
Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys
inferredcites →https://doi.org/10.1016/j.msea.2018.09.048openalex-snapshot
Effect of vanadium content on hydrogen diffusion behaviors and hydrogen induced ductility loss of X80 pipeline steel
inferredcites →https://doi.org/10.1016/j.msea.2020.139598openalex-snapshot
The effect of precipitations (NbC and carbide) in Fe–C–Mn-xNb steels on hydrogen embrittlement characteristics
inferredcites →https://doi.org/10.1016/j.msea.2020.139850openalex-snapshot
Environmental hydrogen embrittlement associated with decohesion and void formation at soluble coarse particles in a cold-rolled Al–Cu based alloy
inferredcites →https://doi.org/10.1016/j.msea.2021.141347openalex-snapshot
Vanadium or copper alloyed duplex lightweight steelwith enhanced hydrogen embrittlement resistance at room temperature
inferredcites →https://doi.org/10.1016/j.msea.2021.142043openalex-snapshot
Hydrogen embrittlement fracture mechanism of 430 ferritic stainless steel: The significant role of carbides and dislocations
inferredcites →https://doi.org/10.1016/j.mspro.2014.06.190openalex-snapshot
Hydrogen Embrittlement of Low Carbon Structural Steel
inferredcites →https://doi.org/10.1016/j.mtla.2020.100626openalex-snapshot
The role of ultrasonic nanocrystalline surface modification at elevated temperature on the hydrogen charging behavior of high-Mn steels
inferredcites →https://doi.org/10.1016/j.prostr.2018.12.231openalex-snapshot
Atomistic modelling of light-element co-segregation at structural defects in iron
inferredcites →https://doi.org/10.1016/j.scriptamat.2004.06.002openalex-snapshot
Hall–Petch relation and boundary strengthening
inferredcites →https://doi.org/10.1016/j.scriptamat.2007.12.023openalex-snapshot
Effect of laser peening on the hydrogen compatibility of corrosion-resistant nickel alloy
inferredcites →https://doi.org/10.1016/j.scriptamat.2010.03.012openalex-snapshot
The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography
inferredcites →https://doi.org/10.1016/j.scriptamat.2011.12.015openalex-snapshot
Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel
inferredcites →https://doi.org/10.1016/j.scriptamat.2014.10.030openalex-snapshot
Improved resistance to hydrogen embrittlement in a high-strength steel by quenching–partitioning–tempering treatment
inferredcites →https://doi.org/10.1016/j.scriptamat.2016.05.012openalex-snapshot
Martensitic transformation-induced hydrogen desorption characterized by utilizing cryogenic thermal desorption spectroscopy during cooling
inferredcites →https://doi.org/10.1016/j.scriptamat.2018.09.043openalex-snapshot
Changing the interfacial composition of carbide precipitates in metals and its effect on hydrogen trapping
inferredcites →https://doi.org/10.1016/j.scriptamat.2022.115043openalex-snapshot
Improvement of resistance against hydrogen embrittlement by controlling carbon segregation at prior austenite grain boundary in 3Mn-0.2C martensitic steels
inferredcites →https://doi.org/10.1016/j.surfcoat.2017.08.037openalex-snapshot
Influence of laser peening on the hydrogen embrittlement resistance of 316L stainless steel
inferredcites →https://doi.org/10.1016/s0013-7944(00)00124-7openalex-snapshot
Hydrogen-induced intergranular fracture of steels
inferredcites →https://doi.org/10.1016/s1359-6454(02)00575-xopenalex-snapshot
Atomistic simulations of effect of hydrogen on kink-pair energetics of screw dislocations in bcc iron
inferredcites →https://doi.org/10.1016/s1359-6454(99)00156-1openalex-snapshot
Hydrogen effects on the character of dislocations in high-purity aluminum
inferredcites →https://doi.org/10.1016/s1359-6454(99)00392-4openalex-snapshot
Deformation-induced defects controlling fracture toughness of steel revealed by tritium desorption behaviors
inferredcites →https://doi.org/10.1016/s1359-6462(96)00440-xopenalex-snapshot
Evidence that carbide precipitation produces hydrogen traps in Ni-17Cr-8Fe alloys
inferredcites →https://doi.org/10.1016/s1359-6462(98)00436-9openalex-snapshot
Deformation induced defects in iron revealed by thermal desorption spectroscopy of tritium
inferredcites →https://doi.org/10.1038/ncomms7164openalex-snapshot
The dual role of coherent twin boundaries in hydrogen embrittlement
inferredcites →https://doi.org/10.1038/s41467-018-05549-yopenalex-snapshot
Crystallographic character of grain boundaries resistant to hydrogen-assisted fracture in Ni-base alloy 725
inferredcites →https://doi.org/10.1038/s41467-019-08752-7openalex-snapshot
Ti and its alloys as examples of cryogenic focused ion beam milling of environmentally-sensitive materials
inferredcites →https://doi.org/10.1038/s41563-021-01050-yopenalex-snapshot
Chemical heterogeneity enhances hydrogen resistance in high-strength steels
inferredcites →https://doi.org/10.1038/s41586-021-04343-zopenalex-snapshot
Hydrogen trapping and embrittlement in high-strength Al alloys
inferredcites →https://doi.org/10.1038/s41598-019-41436-2openalex-snapshot
Comparative study on the effects of Cr, V, and Mo carbides for hydrogen-embrittlement resistance of tempered martensitic steel
inferredcites →https://doi.org/10.1038/s41598-020-58834-6openalex-snapshot
Hydrogen-accelerated spontaneous microcracking in high-strength aluminium alloys
inferredcites →https://doi.org/10.1063/1.1878333openalex-snapshot
The Hydrogen Economy
inferredcites →https://doi.org/10.1073/pnas.2110139119openalex-snapshot
The dual role of martensitic transformation in fatigue crack growth
inferredcites →https://doi.org/10.1080/09500830500482316openalex-snapshot
Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure
inferredcites →https://doi.org/10.1080/09506608.2022.2153220openalex-snapshot
Physical metallurgy of medium-Mn advanced high-strength steels
inferredcites →https://doi.org/10.1088/0965-0393/19/6/065004openalex-snapshot
QM/MM study of dislocation—hydrogen/helium interactions in α-Fe
inferredcites →https://doi.org/10.1098/rspl.1874.0024openalex-snapshot
II. On some remarkable changes produced in iron and steel by the action of hydrogen and acids
inferredcites →https://doi.org/10.1126/science.aal2418openalex-snapshot
Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel
inferredcites →https://doi.org/10.1126/science.aaz0122openalex-snapshot
Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates
inferredcites →https://doi.org/10.1146/annurev.matsci.36.090804.094451openalex-snapshot
HYDROGEN IN METALS: Microstructural Aspects
inferredcites →https://doi.org/10.1179/000844309794239107openalex-snapshot
Precipitate Volume Fraction Estimation in High Strength Microalloyed Steels
inferredcites →https://doi.org/10.1179/174327805x29822openalex-snapshot
Hydrogen re-embrittlement of high strength steel by corrosion of cadmium and aluminium based sacrificial coatings
inferredcites →https://doi.org/10.1515/corrrev-2012-0502openalex-snapshot
Hydrogen embrittlement phenomena and mechanisms
inferredcites →https://doi.org/10.1533/9780857093899.3.493openalex-snapshot
Hydrogen trapping phenomena in martensitic steels
inferredcites →https://doi.org/10.1533/9780857093899.3.707openalex-snapshot
Hydrogen embrittlement of aluminum and aluminum-based alloys
inferredcites →https://doi.org/10.1557/jmr.2017.351openalex-snapshot
Hydrogen embrittlement behaviors of ultrafine-grained 22Mn–0.6C austenitic twinning induced plasticity steel
inferredcites →https://doi.org/10.2139/ssrn.3391563openalex-snapshot
Transformation-Assisted Hydrogen Desorption During Deformation in Steels: Examples of α´- and ε-Martensite
inferredcites →https://doi.org/10.2355/isijinternational.43.527openalex-snapshot
Hydrogen Trapping Behavior in Vanadium-added Steel
inferredcites →https://doi.org/10.2355/isijinternational.isijint-2015-430openalex-snapshot
Prevention of Hydrogen Embrittlement in Steels
inferredcites →https://doi.org/10.2355/isijinternational1966.25.62openalex-snapshot
Role of Carbon in Preventing the Intergranular Fracture in Iron-Phosphorus Alloys
inferredcites →https://doi.org/10.31979/etd.8btb-jqy5openalex-snapshot
Investigation of laser peening effects on hydrogen charged stainless steels
inferredcites →https://doi.org/10.3390/ma13122839openalex-snapshot
Effect of Tempering Temperature after Thermo-Mechanical Control Process on Microstructure Characteristics and Hydrogen-Induced Ductility Loss in High-Vanadium X80 Pipeline Steel

What points at this work

Incoming claims: where this work appears in other papers’ reference lists and arguments.

inferred← citeshttps://doi.org/10.2139/ssrn.4772930openalex-extracted
On the Role of Niobium on Hydrogen Embrittlement of Api 5l X70 and X80 Steels Evaluated by Slow Strain Rate Tensile Testing
inferred← citeshttps://doi.org/10.1002/adem.202401561openalex-snapshot
The Effect of Grain Boundary Misorientation on Hydrogen Flux Using a Phase‐Field‐Based Diffusion and Trapping Model
inferred← citeshttps://doi.org/10.1002/pc.29872openalex-snapshot
Current progress, challenges, and future prospects in composite cryogenic hydrogen storage tanks
inferred← citeshttps://doi.org/10.1007/s11085-025-10358-yopenalex-snapshot
A Comprehensive Review of Corrosion Failure Mechanisms in Advanced Materials: Microscopic Insights and Durability Under Extreme Conditions
inferred← citeshttps://doi.org/10.1007/s11223-024-00705-wopenalex-snapshot
Effect of Stress Concentrations on the Mechanical Properties of Fe-Cr-Ni Steels and Alloys in Gaseous Hydrogen at High Pressures and Temperatures
inferred← citeshttps://doi.org/10.1007/s11661-025-07688-6openalex-snapshot
Hydrogen Effects on Hall–Petch Coefficient and Fracture Strength in Pure Ni and Ni-20Cr Alloy: A Macroscopic Insight of the Hydrogen Embrittlement Mechanism
inferred← citeshttps://doi.org/10.1007/s13272-025-00889-0openalex-snapshot
Analysis of specific failure conditions in electrified propulsion systems using cryogenic hydrogen as a primary energy carrier
inferred← citeshttps://doi.org/10.1016/j.actamat.2026.122495openalex-snapshot
Strengthening and hydrogen-embrittlement resistance via in situ TiC reprecipitation in an additively manufactured high-entropy alloy
inferred← citeshttps://doi.org/10.1016/j.adapen.2024.100168openalex-snapshot
Current challenges in the utilization of hydrogen energy-a focused review on the issue of hydrogen-induced damage and embrittlement
inferred← citeshttps://doi.org/10.1016/j.corsci.2024.112468openalex-snapshot
Synergic effects of temperature and pressure on the hydrogen diffusion and dissolution behaviour of X80 pipeline steel
inferred← citeshttps://doi.org/10.1016/j.corsci.2024.112471openalex-snapshot
Advancing the hydrogen tolerance of ultrastrong aluminum alloys via nanoprecipitate modification
inferred← citeshttps://doi.org/10.1016/j.corsci.2025.113315openalex-snapshot
Superior hydrogen embrittlement resistance of 1.9 GPa-grade precipitation hardening stainless steel achieved by multi-phase precipitation engineering
inferred← citeshttps://doi.org/10.1016/j.corsci.2026.114219openalex-snapshot
Improving the hydrogen embrittlement resistance of a 18Cr ferrite-austenite-martensite triplex stainless steel by copper alloying
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2024.108898openalex-snapshot
Very high-cycle fatigue behavior of steel in hydrogen environment: State of the art review and challenges
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2024.11.166openalex-snapshot
Segregation at prior austenite grain boundaries: The competition between boron and hydrogen
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2025.04.044openalex-snapshot
Investigation of the through-thickness hydrogen embrittlement inhomogeneity in X65 seamless pipeline steel
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2025.151666openalex-snapshot
Hydrogen barrier coatings: Application and assessment
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2025.152737openalex-snapshot
Hydrogen embrittlement mitigation by surface modification: A review on current advances and future perspectives
inferred← citeshttps://doi.org/10.1016/j.ijmecsci.2026.112085openalex-snapshot
The interplay between thermomigration and stress-driven hydrogen transport in metals
inferred← citeshttps://doi.org/10.1016/j.ijpvp.2026.105805openalex-snapshot
Effects of oxygen level and temperature on hydrogen embrittlement behavior of API pipeline steels
inferred← citeshttps://doi.org/10.1016/j.jmrt.2025.01.219openalex-snapshot
Enhancing sulfide stress cracking resistance of a Cu-bearing high strength low alloyed steel through decreasing austenitizing temperature
inferred← citeshttps://doi.org/10.1016/j.jmst.2026.05.023openalex-snapshot
Grain heterogeneity-dislocation synergy on hydrogen embrittlement resistance in medium Mn steel by neutron diffraction
inferred← citeshttps://doi.org/10.1016/j.msea.2025.149119openalex-snapshot
Dual heterogeneous structures enhance the strength and hydrogen embrittlement resistance in CoCrNi-based medium-entropy alloy
inferred← citeshttps://doi.org/10.1016/j.msea.2026.149892openalex-snapshot
The role of carbides in hydrogen permeation behaviour and mechanical degradation of aerospace 4340 and 300M steels
inferred← citeshttps://doi.org/10.1016/j.mtcomm.2025.111997openalex-snapshot
A high-throughput molecular dynamics study with a machine-learning method on predicting diffusion coefficient of hydrogen in α-iron grain boundaries
inferred← citeshttps://doi.org/10.1016/j.mtcomm.2025.113019openalex-snapshot
Fast probe of hydrogen molecules binding on alpha-iron surface via a machine-learning method and high-throughput molecular dynamics simulations
inferred← citeshttps://doi.org/10.1016/j.mtsust.2025.101282openalex-snapshot
Hydrogen embrittlement in storage tank materials and welded joints
inferred← citeshttps://doi.org/10.1016/j.prostr.2025.08.040openalex-snapshot
Hydrogen Embrittlement Susceptibility in High Strength Aerospace Structural Steels
inferred← citeshttps://doi.org/10.1016/j.scriptamat.2025.116789openalex-snapshot
Mitigating hydrogen embrittlement in a 1.8 GPa-grade press-hardened steel by internal stress relaxation via low-temperature tempering
inferred← citeshttps://doi.org/10.1021/acs.chemrev.3c00624openalex-snapshot
Hydrogen Embrittlement as a Conspicuous Material Challenge─Comprehensive Review and Future Directions
inferred← citeshttps://doi.org/10.1111/ffe.14173openalex-snapshot
Guest editorial of virtual special issue: Structural integrity in the context of carbon neutrality
inferred← citeshttps://doi.org/10.1631/jzus.a2300620openalex-snapshot
State-of-the-art and knowledge gaps in gaseous hydrogen pipelines: from the perspective of materials, design, and integrity management
inferred← citeshttps://doi.org/10.2139/ssrn.5357293openalex-snapshot
Improvement on Sulfide Stress Cracking Resistance of a High-Strength Low-Alloyed Steel Via Cu&V Multi-Alloying
inferred← citeshttps://doi.org/10.35860/iarej.1414085openalex-snapshot
A Review on hydrogen embrittlement behavior of steel structures and measurement methods
Editorial review for independent work. ICSAC — the Institute for Complexity Science and Advanced Computing — runs a structured editorial panel for researchers publishing outside journals, and publishes on CiteStamp rails. Submission is free and goes through ORCID: icsacinstitute.org/submit.