The Impact of Impurity Gases on the Hydrogen Embrittlement Behavior of Pipeline Steel in High-Pressure H2 Environments

0 signed · 78 inferred · view as graph

Inferred edges come from two machine sources: sweeps of open repository metadata (mostly SSRN and Zenodo), and a bulk OpenAlex citation snapshot. Every row below is labelled with the one it came from. Neither is a complete citation index — absence here is not evidence of absence.

Is this your work? Sign in with ORCID and put your name on the claims that are yours.
Claim with ORCID
Reference health. See whether every reference in this work resolves to a known work and none has been retracted — and get a dated CiteStamped badge you can embed.
See reference health

What this work says

Outgoing claims: the papers this work cites, builds on, or argues with.

inferredcites →https://doi.org/10.1002/ese3.1500openalex-snapshot
Computational fluid dynamic analysis of hydrogen‐injected natural gas for mixing and transportation behaviors in pipeline structures
inferredcites →https://doi.org/10.1007/s10704-010-9560-zopenalex-snapshot
Influence of hydrogen and frequency on fatigue crack growth behavior of Cr-Mo steel
inferredcites →https://doi.org/10.1007/s10704-012-9783-2openalex-snapshot
Small fatigue crack growth characteristics and fracture surface morphology of low carbon steel in hydrogen gas
inferredcites →https://doi.org/10.1007/s11661-020-05860-8openalex-snapshot
Characteristic Dependency of Hydrogen-Affected Fatigue Crack Growth and Crack Tip Plasticity on Low Loading Frequency in α-Iron
inferredcites →https://doi.org/10.1007/s11837-022-05559-8openalex-snapshot
Feasibility of the Use of Gas Phase Inhibition of Hydrogen Embrittlement in Gas Transmission Pipelines Carrying Hydrogen: A Review
inferredcites →https://doi.org/10.1016/j.actamat.2013.07.001openalex-snapshot
Elucidating the variables affecting accelerated fatigue crack growth of steels in hydrogen gas with low oxygen concentrations
inferredcites →https://doi.org/10.1016/j.actamat.2022.118660openalex-snapshot
Hydrogen-prompted heterogeneous development of dislocation structure in Ni
inferredcites →https://doi.org/10.1016/j.apsusc.2023.156871openalex-snapshot
Hydrogen-surface interaction from first-principles calculations and its implication to hydrogen embrittlement mechanisms of titanium
inferredcites →https://doi.org/10.1016/j.corsci.2012.08.015openalex-snapshot
Assessing the effect of low oxygen concentrations in gaseous hydrogen embrittlement of DIN 1.4301 and 1.1200 steels at high gas pressures
inferredcites →https://doi.org/10.1016/j.corsci.2014.07.061openalex-snapshot
Effects of environmental conditions on hydrogen permeation of X52 pipeline steel exposed to high H2S-containing solutions
inferredcites →https://doi.org/10.1016/j.corsci.2022.110594openalex-snapshot
Hydrogen uptake induced by CO2 enhances hydrogen embrittlement of iron in hydrogen blended natural gas
inferredcites →https://doi.org/10.1016/j.egypro.2019.01.887openalex-snapshot
ELEGANCY: The Interdisciplinary Approach of the German Case Study to Enable a Low Carbon Economy by Hydrogen and CCS
inferredcites →https://doi.org/10.1016/j.engfracmech.2011.09.007openalex-snapshot
Effects of hydrogen pressure and test frequency on fatigue crack growth properties of Ni–Cr–Mo steel candidate for a storage cylinder of a 70MPa hydrogen filling station
inferredcites →https://doi.org/10.1016/j.engfracmech.2017.08.014openalex-snapshot
Investigation of cleavage fracture under dynamic loading conditions: Part I fractographic analysis
inferredcites →https://doi.org/10.1016/j.engfracmech.2019.106528openalex-snapshot
The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: Localized plasticity and decohesion
inferredcites →https://doi.org/10.1016/j.heliyon.2023.e21454openalex-snapshot
Study progress on the pipeline transportation safety of hydrogen-blended natural gas
inferredcites →https://doi.org/10.1016/j.ijfatigue.2010.01.006openalex-snapshot
Nanostructurally small cracks (NSC): A review on atomistic modeling of fatigue
inferredcites →https://doi.org/10.1016/j.ijfatigue.2017.04.010openalex-snapshot
Hydrogen trapping and fatigue crack growth property of low-carbon steel in hydrogen-gas environment
inferredcites →https://doi.org/10.1016/j.ijhydene.2022.06.158openalex-snapshot
Research and demonstration on hydrogen compatibility of pipelines: a review of current status and challenges
inferredcites →https://doi.org/10.1016/j.ijhydene.2022.07.261openalex-snapshot
The future of hydrogen energy: Bio-hydrogen production technology
inferredcites →https://doi.org/10.1016/j.ijhydene.2023.02.050openalex-snapshot
Micro-mechanism study on the effect of O2 poisoned ZrCo surface on hydrogen absorption performance
inferredcites →https://doi.org/10.1016/j.ijhydene.2023.04.283openalex-snapshot
Use of existing gas infrastructure in European hydrogen economy
inferredcites →https://doi.org/10.1016/j.ijhydene.2023.12.274openalex-snapshot
An atomistic study on the HELP mechanism of hydrogen embrittlement in pure metal Fe
inferredcites →https://doi.org/10.1016/j.ijhydene.2024.02.245openalex-snapshot
A review of gas phase inhibition of gaseous hydrogen embrittlement in pipeline steels
inferredcites →https://doi.org/10.1016/j.ijhydene.2024.04.116openalex-snapshot
CO2 effect on the fatigue crack growth of X80 pipeline steel in hydrogen-enriched natural gas: Experiment vs DFT
inferredcites →https://doi.org/10.1016/j.ijplas.2024.103890openalex-snapshot
A continuum scale chemo-mechanical model for multi-trap hydrogen transport in deformed polycrystalline metals
inferredcites →https://doi.org/10.1016/j.jmrt.2022.12.004openalex-snapshot
Influence of hydrogen environment on fatigue fracture morphology of X80 pipeline steel
inferredcites →https://doi.org/10.1016/j.mtcomm.2023.107269openalex-snapshot
Effect of loading rate on the dislocation emission from crack-tip under hydrogen environment
inferredcites →https://doi.org/10.1016/j.ngib.2023.11.001openalex-snapshot
Research progress on corrosion and hydrogen embrittlement in hydrogen–natural gas pipeline transportation
inferredcites →https://doi.org/10.1016/j.scriptamat.2020.08.011openalex-snapshot
Enhanced hydrogen embrittlement of low-carbon steel to natural gas/hydrogen mixtures
inferredcites →https://doi.org/10.1016/s0997-7538(01)01179-2openalex-snapshot
Hydrogen induced shear localization of the plastic flow in metals and alloys
inferredcites →https://doi.org/10.1021/acsomega.1c01946openalex-snapshot
Effect of Impurity Atoms on the Adsorption/Dissociation of Hydrogen Sulfide and Hydrogen Diffusion on the Fe(100) Surface
inferredcites →https://doi.org/10.1021/acsomega.3c01131openalex-snapshot
Key Technologies of Pure Hydrogen and Hydrogen-Mixed Natural Gas Pipeline Transportation
inferredcites →https://doi.org/10.1111/ffe.12994openalex-snapshot
Inhibitory effect of oxygen on hydrogen‐induced fracture of A333 pipe steel
inferredcites →https://doi.org/10.1115/1.3225777openalex-snapshot
Treatise on Materials Science and Technology, Vol. 19, Experimental Methods, Part B
inferredcites →https://doi.org/10.1520/stp1020-ebopenalex-snapshot
Fracture Mechanics: Perspectives and Directions (Twentieth Symposium)
inferredcites →https://doi.org/10.1533/9780857093899openalex-snapshot
Gaseous hydrogen embrittlement of materials in energy technologies Volume 1
inferredcites →https://doi.org/10.3390/ma16041741openalex-snapshot
Significance of Melt Pool Structure on the Hydrogen Embrittlement Behavior of a Selective Laser-Melted 316L Austenitic Stainless Steel
inferredcites →https://doi.org/10.3390/ma16175799openalex-snapshot
Modeling Corrosion Product Film Formation and Hydrogen Diffusion at the Crack Tip of Austenitic Stainless Steel
inferredcites →https://doi.org/10.3390/ma16206680openalex-snapshot
An Overview of Challenges for the Future of Hydrogen
inferredcites →https://doi.org/10.3390/ma17040965openalex-snapshot
Hydrogen Impact: A Review on Diffusibility, Embrittlement Mechanisms, and Characterization
inferredcites →https://doi.org/10.3390/met12061032openalex-snapshot
Analysis of Hydrogen-Assisted Brittle Fracture Using Phase-Field Damage Modelling Considering Hydrogen Enhanced Decohesion Mechanism
inferredcites →https://doi.org/10.3390/pr11113180openalex-snapshot
Research Progress and Prospects on Hydrogen Damage in Welds of Hydrogen-Blended Natural Gas Pipelines

What points at this work

Incoming claims: where this work appears in other papers’ reference lists and arguments.

inferred← citeshttps://doi.org/10.2139/ssrn.5081019openalex-extracted
Effect of Dynamic Charging and Pre-Charging Hydrogen on the Fracture Properties of Gb20# and X80 Steels
inferred← citeshttps://doi.org/10.1007/978-981-95-5609-0_4openalex-snapshot
Materials for Hydrogen Pipeline Applications
inferred← citeshttps://doi.org/10.1007/978-981-95-5609-0_5openalex-snapshot
Pipeline Design Considerations for Hydrogen
inferred← citeshttps://doi.org/10.1007/s11340-026-01339-6openalex-snapshot
High-Sensitivity Hydrogen Gas Permeation: System Development, Sample Preparation, and Influence of Testing Variables
inferred← citeshttps://doi.org/10.1007/s11665-025-11871-6openalex-snapshot
Evaluation of Mechanical Properties and Fatigue Performance of L450 Pipeline Steel Base Metal and Welds
inferred← citeshttps://doi.org/10.1007/s40195-024-01755-4openalex-snapshot
Using Small Punch Test to Investigate the Mechanical Properties of X42 Exposed to Gaseous Hydrogen: Effect of Pressure, Pre-charge Time, Punch Velocity and Oxygen Content
inferred← citeshttps://doi.org/10.1016/j.commatsci.2025.114308openalex-snapshot
A study on the adsorption and diffusion of H2S on pipeline steel surfaces and the influence of passive film defects on hydrogen diffusion behavior based on first principles
inferred← citeshttps://doi.org/10.1016/j.corsci.2024.112580openalex-snapshot
Determination of the hydrogen fugacity during cathodic hydrogen charging of X65 D pipeline steel
inferred← citeshttps://doi.org/10.1016/j.corsci.2025.113555openalex-snapshot
The influence of CO2 partial pressure on the hydrogen embrittlement behavior of pure iron in high-pressure hydrogen environment
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2025.109410openalex-snapshot
Hydrogen embrittlement in vintage grade 290 pipeline steel and its welded region via ex-situ and in-situ testing
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2025.109964openalex-snapshot
Impacts of gas composition and temperature on the hydrogen embrittlement of pipeline steels
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2026.111307openalex-snapshot
Comprehending the inhibitory effects of oxygen and carbon monoxide on the hydrogen embrittlement of pipeline steel via both experimental investigation and simulation calculation
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2025.04.333openalex-snapshot
Advances and prospects of failure modes in key hydrogen-related components within the hydrogen energy supply chain
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2025.150459openalex-snapshot
Gaseous hydrogen permeation in X65 D pipeline steel and a preliminary evaluation of the influence of oxygen
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2026.154218openalex-snapshot
Hydrogen embrittlement in the hydrogen economy: A review of metal material challenges and mitigation strategies for carbon neutrality
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2026.154861openalex-snapshot
Complex interplay of co-existing gas impurities and their effects on hydrogen embrittlement in metallic materials: A comprehensive review
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2026.156142openalex-snapshot
Understanding the role of oxygen in preventing hydrogen embrittlement in pipeline steels
inferred← citeshttps://doi.org/10.1016/j.ijpvp.2026.105805openalex-snapshot
Effects of oxygen level and temperature on hydrogen embrittlement behavior of API pipeline steels
inferred← citeshttps://doi.org/10.1016/j.jmrt.2025.07.269openalex-snapshot
Investigation of hydrogen embrittlement in steel alloys: mechanism, factors, advanced methods and materials, applications, challenges, and future directions: A review
inferred← citeshttps://doi.org/10.1016/j.jpse.2025.100284openalex-snapshot
Effect of gas impurities on the dissociative adsorption of hydrogen on Fe(100) surface of pipeline steel
inferred← citeshttps://doi.org/10.1016/j.jpse.2026.100487openalex-snapshot
Non-additive effects of CO and H2O impurities on H2 dissociation and subsurface diffusion on Fe(110): A first-principles study
inferred← citeshttps://doi.org/10.1016/j.jpse.2026.100588openalex-snapshot
Fracture Evolution and Control of Supercritical/Dense CO2 Pipelines under Thermal-Fluid-Chemical-Mechanical (TFCM) Coupling: A Review of Initiation, Propagation, and Arrest Mechanisms
inferred← citeshttps://doi.org/10.1016/j.memsci.2025.123967openalex-snapshot
Pre-assembly and post-annealing of ZIF-7-NH2-based mixed matrix membranes for improved interfacial compatibility
inferred← citeshttps://doi.org/10.1016/j.tafmec.2026.105821openalex-snapshot
A unified phase-field framework for coupled oxygen-assisted corrosion, hydrogen embrittlement, and fracture evolution
inferred← citeshttps://doi.org/10.1088/1742-6596/3143/1/012086openalex-snapshot
Sealing performance of pipes and joints in pure hydrogen
inferred← citeshttps://doi.org/10.1108/acmm-10-2025-3419openalex-snapshot
Comparison of hydrogen embrittlement in the coarse-grained heat-affected zone of X52 and X65 steels fabricated by GMAW, CMT and FCAW
inferred← citeshttps://doi.org/10.1111/ffe.70367openalex-snapshot
Effect of High‐Pressure Natural Gas/Hydrogen Mixed Environment on the Fatigue Life of X65 Pipeline Steel Welded Joints
inferred← citeshttps://doi.org/10.1155/adv/2715691openalex-snapshot
Comprehensive Evaluation of NBR Sealing Performance Under Medium‐Pressure Hydrogen Aging: Experimental Analysis and Predictive Model Using Convolutional Neural Network
inferred← citeshttps://doi.org/10.2139/ssrn.7477422openalex-snapshot
Hydrogen surface activation, trapping, and oxygen inhibition in ARMCO iron and X70 studied using gaseous hydrogen permeation
inferred← citeshttps://doi.org/10.3389/fchem.2026.1957974openalex-snapshot
Mechanisms of hydrogen embrittlement, mitigation strategies, and emerging materials for hydrogen energy and advanced manufacturing
inferred← citeshttps://doi.org/10.3390/ma18174139openalex-snapshot
Effect of Copper Alloying on Hydrogen Embrittlement of Fe-28Mn-10Al-1C Austenitic Low-Density Steel
inferred← citeshttps://doi.org/10.3390/met15101123openalex-snapshot
Mechanical Testing Methods for Assessing Hydrogen Embrittlement in Pipeline Steels: A Review
inferred← citeshttps://doi.org/10.3390/met16080828openalex-snapshot
Experimental Investigation of Hydrogen-Assisted Fatigue Crack Growth in Vintage X52 and X70 Pipeline Steels Under Hydrogen–Natural Gas Blending
inferred← citeshttps://doi.org/10.5006/ac2026_00026openalex-snapshot
Develop Testing Methods for Evaluating Hydrogen Embrittlement Mitigation Approaches Based on Thermal Desorption Mass Spectrometry (TDMS)
inferred← citeshttps://doi.org/10.5772/intechopen.1008391openalex-snapshot
Enhancing Pipeline Reliability: A Structural Integrity Management Approach Using Minimal Cut Set Method and Importance Measures
Editorial review for independent work. ICSAC — the Institute for Complexity Science and Advanced Computing — runs a structured editorial panel for researchers publishing outside journals, and publishes on CiteStamp rails. Submission is free and goes through ORCID: icsacinstitute.org/submit.