An Assessment of the High-Temperature Oxidation Behavior of Fe-Cr Steels in Water Vapor and Steam

0 signed · 62 inferred · view as graph

Inferred edges come from two machine sources: sweeps of open repository metadata (mostly SSRN and Zenodo), and a bulk OpenAlex citation snapshot. Every row below is labelled with the one it came from. Neither is a complete citation index — absence here is not evidence of absence.

Is this your work? Sign in with ORCID and put your name on the claims that are yours.
Claim with ORCID
Reference health. See whether every reference in this work resolves to a known work and none has been retracted — and get a dated CiteStamped badge you can embed.
See reference health

What this work says

Outgoing claims: the papers this work cites, builds on, or argues with.

inferredcites →https://doi.org/10.1002/9780470549070.ch4openalex-snapshot
Materials Performance
inferredcites →https://doi.org/10.1007/bf00541841openalex-snapshot
55Fe diffusion in magnetite crystals at 500� C and its relevance to oxidation of iron
inferredcites →https://doi.org/10.1007/bf00603656openalex-snapshot
Stratified oxide scale growth on two Cr-Ni steels oxidized in high-pressure steam at 800�C
inferredcites →https://doi.org/10.1007/bf00604478openalex-snapshot
A study of the Cr-depleted surface layers formed on four Cr-Ni steels during oxidation in steam at 600� C and 800� C
inferredcites →https://doi.org/10.1007/bf00664425openalex-snapshot
Observation of oscillating reaction rates during the isothermal oxidation of ferritic steels
inferredcites →https://doi.org/10.1007/bf00665267openalex-snapshot
Internal-external transition for the oxidation of Fe-Cr-Ni austenitic stainless steels in steam
inferredcites →https://doi.org/10.1007/bf00666721openalex-snapshot
Kinetics of oxidation of ferrous alloys by super-heated steam
inferredcites →https://doi.org/10.1016/0010-938x(81)90024-xopenalex-snapshot
The effect of grain size on the corrosion behaviour of inconel 600 in high-temperature steam
inferredcites →https://doi.org/10.1016/0010-938x(82)90037-3openalex-snapshot
High temperature corrosion
inferredcites →https://doi.org/10.1016/s0010-938x(69)80083-1openalex-snapshot
Gas phase transport in the oxidation of Fe and steel
inferredcites →https://doi.org/10.1016/s0022-3115(00)00248-8openalex-snapshot
A microstructural study of the oxide scale formation on ODS Fe–13Cr steel
inferredcites →https://doi.org/10.1023/a:1004610626903openalex-snapshot
Hydrogen in Chromium: Influence on the High-Temperature Oxidation Kinetics in H2O, Oxide-Growth Mechanisms, and Scale Adherence
inferredcites →https://doi.org/10.1119/1.10975openalex-snapshot
Teaching megalithic astronomy
inferredcites →https://doi.org/10.1149/1.2423661openalex-snapshot
Effect of Surface Treatment on the Corrosion of Stainless Steels in High-Temperature Water and Steam
inferredcites →https://doi.org/10.1149/1.2425229openalex-snapshot
The Oxidation of an Iron-5 Per Cent Chromium Alloy in the Temperature Range 600°–850°C
inferredcites →https://doi.org/10.1149/1.2425624openalex-snapshot
Oxide Structures Produced on Iron-Chromium Alloys by a Dissociative Mechanism
inferredcites →https://doi.org/10.1149/1.2425932openalex-snapshot
Corrosion of Steels and Nickel Alloys in Superheated Steam
inferredcites →https://doi.org/10.1149/1.2425963openalex-snapshot
The Mechanism of the High-Temperature Oxidation of Iron-Chromium Alloys in Water Vapor
inferredcites →https://doi.org/10.2355/tetsutohagane1955.74.5_863openalex-snapshot
High Temperature Oxidation of Fe-Cr Alloys in Ar-10% H2O Atmosphere
inferredcites →https://doi.org/10.5006/0010-9312-18.10.368openalex-snapshot
Corrosion of Carbon Steel and Other Steels In Simulated Boiling-Water Reactor Environment: Phase II
inferredcites →https://doi.org/10.5006/0010-9312-21.8.260openalex-snapshot
Corrosion of Carbon Steel in Simulated Boiling Water and Superheat Reactor Environments
inferredcites →https://doi.org/10.5006/1.3585251openalex-snapshot
Scaling of Austenitic Stainless Steels and Nickel-Base Alloys in High-Temperature Steam at 973 K

What points at this work

Incoming claims: where this work appears in other papers’ reference lists and arguments.

inferred← citeshttps://doi.org/10.2139/ssrn.4864963openalex-extracted
Prolonged High-Temperature Oxidation Failure Models of Fe-Cr Alloys: Investigating the Mechanisms of Fe3o4 Layer Fracture
inferred← citeshttps://doi.org/10.1002/9781119027973.ch19openalex-snapshot
Effect of Alloying Additions on Oxidation Behaviors of Ni‐Fe Based Superalloy for Ultra‐Supercritical Boiler Applications
inferred← citeshttps://doi.org/10.1007/978-3-319-48765-6_19openalex-snapshot
Effect of Alloying Additions on Oxidation Behaviors of Ni-Fe Based Superalloy for Ultra-Supercritical Boiler Applications
inferred← citeshttps://doi.org/10.1007/s11085-014-9474-7openalex-snapshot
Oxidation of Ferritic Steel T24 in Supercritical Water
inferred← citeshttps://doi.org/10.1007/s11665-025-13117-xopenalex-snapshot
Effect of Cr Concentration on the Structural Properties, Hardness and Oxidation Behavior of Fe-Cr-Ti Ferritic Alloys
inferred← citeshttps://doi.org/10.1007/s11668-019-00662-6openalex-snapshot
Research on Remaining Life Evaluation Method of T92 Steel for Superheater Tube Based on Oxide Layer Growth
inferred← citeshttps://doi.org/10.1007/s11837-006-0061-5openalex-snapshot
Materials for high-temperature protection
inferred← citeshttps://doi.org/10.1016/b978-0-12-819921-3.00008-xopenalex-snapshot
Harmful phenomena in modernized boilers
inferred← citeshttps://doi.org/10.1016/j.applthermaleng.2025.125953openalex-snapshot
A comprehensive model for the prediction of boiler platen superheater tube temperature considering the effects of ash deposits and oxide scale
inferred← citeshttps://doi.org/10.1016/j.corsci.2008.08.024openalex-snapshot
Corrosion behavior of Ni-base alloys for advanced high temperature water-cooled nuclear plants
inferred← citeshttps://doi.org/10.1016/j.corsci.2009.03.008openalex-snapshot
Oxidation of 316 stainless steel in supercritical water
inferred← citeshttps://doi.org/10.1016/j.corsci.2009.12.032openalex-snapshot
Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water
inferred← citeshttps://doi.org/10.1016/j.corsci.2011.03.015openalex-snapshot
Impact of oxyfuel atmospheres H2O/CO2/O2 and H2O/CO2 on the oxidation of ferritic–martensitic and austenitic steels
inferred← citeshttps://doi.org/10.1016/j.corsci.2015.10.017openalex-snapshot
Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water
inferred← citeshttps://doi.org/10.1016/j.corsci.2020.108852openalex-snapshot
Long-term corrosion performance of T91 ferritic/martensitic steel at 400 °C in flowing Pb-Bi eutectic with 2 × 10−7 mass% dissolved oxygen
inferred← citeshttps://doi.org/10.1016/j.enconman.2021.114166openalex-snapshot
Co-production of hydrogen and syngas from chemical looping water splitting coupled with decomposition of glycerol using Fe-Ce-Ni based oxygen carriers
inferred← citeshttps://doi.org/10.1016/j.engfailanal.2011.09.001openalex-snapshot
The rate of corrosive wear in superheaters of boilers for supercritical parameters of steam
inferred← citeshttps://doi.org/10.1016/j.icheatmasstransfer.2025.108664openalex-snapshot
Prediction of the tube temperature and oxide scale formation of boiler superheater by a coupled combustion and hydrodynamic model
inferred← citeshttps://doi.org/10.1016/j.ijhydene.2010.04.099openalex-snapshot
High-temperature oxidation performance of a new alumina-forming Ni–Fe–Cr–Al alloy in flowing air
inferred← citeshttps://doi.org/10.1016/j.jnucmat.2007.05.001openalex-snapshot
Corrosion behavior of a ferritic/martensitic steel HCM12A exposed to harsh environments
inferred← citeshttps://doi.org/10.1016/j.matchemphys.2019.122443openalex-snapshot
Micro-structural evolution of oxide scales formed on a Nb-Stabilizing heat-resistant steel at the initial stage in high-temperature water vapor
inferred← citeshttps://doi.org/10.1016/j.supflu.2016.10.002openalex-snapshot
A comparative study on the oxidation of austenitic alloys 304 and 304-oxide dispersion strengthened steel in supercritical water at 650 °C
inferred← citeshttps://doi.org/10.1016/j.supflu.2025.106663openalex-snapshot
Synergistic corrosion mechanisms of supercritical water and Na2SO4 deposition layer: Austenitic stainless steels 316 L and 304
inferred← citeshttps://doi.org/10.1080/09603409.2017.1286549openalex-snapshot
Oxidation of low-alloy steel in high temperature steam and supercritical water
inferred← citeshttps://doi.org/10.1080/09603409.2018.1468524openalex-snapshot
High temperature oxidation behavior of ferritic steel in supercritical water at 550–700°C
inferred← citeshttps://doi.org/10.1080/1478422x.2016.1185568openalex-snapshot
Impact specimen geometry on T23 and TP347HFG steels behaviour during steam oxidation at harsh conditions
inferred← citeshttps://doi.org/10.1088/1757-899x/329/1/012010openalex-snapshot
High temperature coatings from post processing Fe-based chips and Ni-based alloys as a solution for critical raw materials
inferred← citeshttps://doi.org/10.1115/1.4031338openalex-snapshot
Supercritical Oxidation of Boiler Tube Materials
inferred← citeshttps://doi.org/10.1115/1.4053379openalex-snapshot
Effect of Shot Peening on the Surface Oxidation of P92 Steel in the Steam Environment at 600 °C
inferred← citeshttps://doi.org/10.1179/1743278214y.0000000222openalex-snapshot
Steam oxidation of TP347HFG, super 304H and HR3C – analysis of significance of steam flowrate and specimen surface finish
inferred← citeshttps://doi.org/10.1361/105994906x108756openalex-snapshot
Boiler Materials for Ultra-Supercritical Coal Power Plants—Steamside Oxidation
inferred← citeshttps://doi.org/10.2172/833921openalex-snapshot
BOILER MATERIALS FOR ULTRASUPERCRITICAL COAL POWER PLANTS
inferred← citeshttps://doi.org/10.2172/944040openalex-snapshot
Candidate Materials Evaluation for Supercritical Water-Cooled Reactor
inferred← citeshttps://doi.org/10.2478/kom-2013-0005openalex-snapshot
High-temperature oxidation of high-alloyed steel
inferred← citeshttps://doi.org/10.2478/v10176-012-0026-xopenalex-snapshot
Rate of corrosion of waterwalls in supercritical pulverised fuel boilers
inferred← citeshttps://doi.org/10.4028/www.scientific.net/amr.516-517.524openalex-snapshot
Study of Forming & Exfoliation Mechanism of Oxide Skin in High-Temperature Tube of Supercritical Boiler
inferred← citeshttps://doi.org/10.5006/1.3278410openalex-snapshot
Corrosion Behavior of Alloys 625 and 718 in Supercritical Water
inferred← citeshttps://doi.org/10.5006/1065openalex-snapshot
Steam Oxidation of 9% to 12%Cr Steels: Critical Evaluation and Implications for Practical Application
inferred← citeshttps://doi.org/10.5006/1859openalex-snapshot
Effect of Surface Condition on Steam Oxidation of Martensitic Steels and Nickel-Based Alloys
inferred← citeshttps://doi.org/10.5006/c2004-04486openalex-snapshot
Supercritical Steam in Power Production—a Materials Review
Editorial review for independent work. ICSAC — the Institute for Complexity Science and Advanced Computing — runs a structured editorial panel for researchers publishing outside journals, and publishes on CiteStamp rails. Submission is free and goes through ORCID: icsacinstitute.org/submit.